PolyOne Synprene® IT 62-001 Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® IT 62-001 Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Over-Molding GradeNaturalTransparentUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Linear Mold Shrinkage 0.0135 cm/cm
0.0135 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
10 Sec; ASTM D2240
60
60
Instant; ASTM D2240
Tensile Strength, Yield 7.481 MPa
1085 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
2.34 MPa

@Strain 100 %
340 psi

@Strain 100 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
4.24 MPa

@Strain 300 %
615 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 670 %
670 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 35.9 kN/m
205 pli
Die C (graves), 20 in/min; ASTM D624
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified