Material Notes:
Application: UL94 V-2, Flame-retardant polypropylene compounds for injection molding applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.910 - 0.950 g/cc
0.910 - 0.950 g/cc
ASTM D792
Melt Flow 20 - 30 g/10 min
20 - 30 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 24.1 MPa
>= 3500 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Modulus >= 1.03 GPa
>= 150 ksi
ASTM D790
Izod Impact, Notched >= 0.107 J/cm
>= 0.200 ft-lb/in
ASTM D256
Dart Drop, Total Energy >= 2.71 J
>= 2.00 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Flammability Test 3.0

@Thickness 0.7937 mm
3.0

@Thickness 0.03125 in
Oxygen Index >= 27 %
>= 27 %
ASTM D2863