Teknor Apex UNIPRENE® 7400-80 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name UNIPRENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex UNIPRENE® 7400-80 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
5 seconds; ASTM D2240
Tensile Strength, Yield 3.79 MPa
550 psi
Adhesion to EPDM, 0.125" Micro Die, 8"/min; ASTM D412
8.62 MPa
1250 psi
ASTM D412
8.62 MPa
1250 psi
100% Retention, Hot Air Aging, 22 hrs at 70°C
Elongation at Break 450 %
450 %
ASTM D412
450 %
450 %
100% Retention, Hot Air Aging, 22 hrs at 70°C
Elongation at Yield 70 %
70 %
Adhesion to EPDM, 0.125" Micro Die, 8"/min; ASTM D412
100% Modulus 0.00483 GPa
0.700 ksi
ASTM D412
Compression Set 37 %
37 %
23°C, 22 hr.; ASTM D395, Method B
51 %
51 %
70°C, 22 hr.; ASTM D395, Method B