| Category | Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Thermoplastic Olefinic Elastomer (TPO) |
| Manufacturer | A. Schulman, Inc. |
| Trade Name | POLYTROPE™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
| Melt Index of Compound | 10 g/10 min | 10 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 66 | 66 | ASTM D2240 |
| Tensile Strength at Break | 24.1 MPa | 3500 psi | ASTM D638 |
| Elongation at Break | 650 % | 650 % | ASTM D638 |
| Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D790 |
| Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -40.0 °C | -40.0 °F |