Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufGuard M™ GPP1005M-CD PP, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer S&E Specialty Polymers
Trade Name TufGuard M™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufGuard M™ GPP1005M-CD PP, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A UL94 V-2, flame retardant polypropylene compound for injection molding applications, including cases for industrial power supply. Compound is designed with halogen-based flame retardant technology and is available in a wide spectrum of colors.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.910 - 0.950 g/cc
0.910 - 0.950 g/cc
ASTM D792
Melt Flow 13.0 - 18.0 g/10 min
13.0 - 18.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 22.8 MPa
>= 3300 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
Ultimate; ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched >= 1.07 J/cm
>= 2.00 ft-lb/in
ASTM D256
Gardner Impact >= 24.4 J
>= 18.0 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 0.7937 mm
V-2

@Thickness 0.03125 in
Oxygen Index >= 25.0 %
>= 25.0 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 2.10

@Frequency 1000 Hz
2.10

@Frequency 1000 Hz
ASTM D1531
Processing Properties Metric English Comments
Processing Temperature 204 - 218 °C
400 - 425 °F
Suggested Stock
Descriptive Properties Value Comments
Mold Shrinkage 13-15 mils/inch