Material Notes:
Notes: RoHS Compliant Uses: Consumer Applications; Gaskets; Medical/Healthcare Applications; Membranes; Packaging; Safety Equipment; Sporting Goods; Tape; Tubing Forms: Pellets Processing Method: Film Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C); Injection Rate: Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 2.00 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.00 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
ASTM D2240
Tensile Strength at Break 11.7 MPa
1700 psi
20 in/min; ASTM D412
Tensile Stress 0.621 MPa

@Strain 100 %
90.0 psi

@Strain 100 %
20 in/min; ASTM D412
Elongation at Break 740 %
740 %
20 in/min; ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 232 °C
360 - 450 °F
Middle Barrel Temperature 188 - 238 °C
370 - 460 °F
Front Barrel Temperature 193 - 243 °C
380 - 470 °F
Nozzle Temperature 199 - 249 °C
390 - 480 °F
Zone 1 182 - 232 °C
360 - 450 °F
Zone 2 188 - 238 °C
370 - 460 °F
Zone 3 193 - 243 °C
380 - 470 °F
Zone 5 199 - 249 °C
390 - 480 °F
Die Temperature 199 - 249 °C
390 - 480 °F
Melt Temperature 199 - 249 °C
390 - 480 °F
Processing Temperature
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Injection Pressure 1.38 - 5.52 MPa
200 - 800 psi
Back Pressure 0.172 - 0.689 MPa
25.0 - 100 psi
Cushion 0.381 - 2.54 cm
0.150 - 1.00 in
Screw Speed 50 - 100 rpm
50 - 100 rpm
Descriptive Properties Value Comments