G-2701 Styrene-based Biomedical Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF G-2701 Styrene-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
ASTM D2240
Tensile Strength, Ultimate 11.0 MPa
1600 psi
ASTM D412
Tensile Strength, Yield 3.31 MPa
480 psi
at 100%; ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
Tear Strength 45.6 kN/m
260 pli
die B; ASTM D624