Material Notes:
Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Flexural Yield Strength 64.8 MPa
9400 psi
ASTM D790
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 108 µm/m-°C

@Temperature 20.0 °C
60.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648