Material Notes:
DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
24 min.; ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 0.930 GPa
135 ksi
880 min.; ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
40 min.; ASTM D256