Chase Plastics CP Pryme® N300HL (Dry) Nylon 6, Heat Stabilized, Lubricated, Recycled Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N300HL (Dry) Nylon 6, Heat Stabilized, Lubricated, Recycled Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Heat StabilizedLubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.8 %
1.8 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.010 - 0.014 cm/cm
0.010 - 0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.90 GPa
420 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
420 °F
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C
150 °F
Unannealed; ASTM D648