Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA

Category Polymer , Thermoplastic , Nylon , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blowmolding and extrusion. High heat and chemical resistant.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.013 - 0.014 cm/cm

@Thickness 3.20 mm
0.013 - 0.014 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 83 %
83 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 95.0 MPa
13800 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.27 GPa
329 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 3.36 J/cm
6.29 ft-lb/in
ASTM D256
1.22 J/cm

@Temperature -30.0 °C
2.29 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Dart Drop, Total Energy 31.0 J
22.9 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
36.0 J

@Temperature -30.0 °C
26.6 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 179 °C

@Thickness 6.40 mm
354 °F

@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical with Impact 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical without Impact 50.0 °C
122 °F
UL 746B
Flammability, UL94 HB

@Thickness 1.49 mm
HB

@Thickness 0.0587 in
UL 94
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved