Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GFT15N050-WBK 15% Glass Fiber Reinforced, Toughened, Weatherable Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GFT15N050-WBK 15% Glass Fiber Reinforced, Toughened, Weatherable Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Fiber Reinforced, Toughened, Weatherable Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183-87
Filler Content 15 %
15 %
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0085 - 0.0105 cm/cm
0.0085 - 0.0105 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ISO 527-93
Elongation at Break 3.0 %
3.0 %
ISO 527-93
Flexural Strength 120 MPa
17400 psi
ISO 178-93
Flexural Modulus 4.25 GPa
616 ksi
ISO 178-93
Izod Impact, Notched (ISO) 12.5 kJ/m²
5.95 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ISO 75-93
Users viewing this material also viewed the following: