Polymer Property : Linear Mold Shrinkage = 0.0100 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0100 - 0.0310 cm/cm
0.0100 - 0.0310 in/in
Average value: 0.0146 cm/cm Grade Count:41
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..
Linear Mold Shrinkage 0.0100 - 0.0250 cm/cm
0.0100 - 0.0250 in/in
Average value: 0.0175 cm/cm Grade Count:4
Overview of materials for Polypropylene, Fiber Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app..
Linear Mold Shrinkage 0.0100 - 0.0350 cm/cm
0.0100 - 0.0350 in/in
Average value: 0.0255 cm/cm Grade Count:29
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.0100 - 0.0500 cm/cm
0.0100 - 0.0500 in/in
Average value: 0.0200 cm/cm Grade Count:8
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage 0.0100 - 0.0200 cm/cm
0.0100 - 0.0200 in/in
Average value: 0.0143 cm/cm Grade Count:14
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
Linear Mold Shrinkage 0.0100 - 0.0300 cm/cm
0.0100 - 0.0300 in/in
Average value: 0.0221 cm/cm Grade Count:20
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage 0.0100 - 0.0180 cm/cm
0.0100 - 0.0180 in/in
Average value: 0.0120 cm/cm Grade Count:33
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.0100 - 0.0130 cm/cm

@Temperature 150 - 150 °C
0.0100 - 0.0130 in/in

@Temperature 302 - 302 °F
Average value: 0.0109 cm/cm Grade Count:17
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.0100 - 0.0130 cm/cm

@Time 900 - 900 sec
0.0100 - 0.0130 in/in

@Time 0.250 - 0.250 hour
Average value: 0.0109 cm/cm Grade Count:17
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.0100 - 0.0250 cm/cm
0.0100 - 0.0250 in/in
Average value: 0.0159 cm/cm Grade Count:16
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.0100 - 0.0250 cm/cm
0.0100 - 0.0250 in/in
Average value: 0.0173 cm/cm Grade Count:7
Overview of materials for Polypropylene, Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage 0.0100 - 0.0400 cm/cm
0.0100 - 0.0400 in/in
Average value: 0.0346 cm/cm Grade Count:102
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.0100 - 0.0200 cm/cm
0.0100 - 0.0200 in/in
Average value: 0.0146 cm/cm Grade Count:13
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..