Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.010 - 0.030 cm/cm | 0.010 - 0.030 in/in | |
Multibase TPSiV® 3111-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Hydrolysis resistant; FDA 21 CFR 177.2600 CompliantAPPLICATIONS: Solution for soft touc.. |
|||
Linear Mold Shrinkage | 0.010 - 0.030 cm/cm | 0.010 - 0.030 in/in | |
Multibase TPSiV® 4000-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Linear Mold Shrinkage | 0.010 - 0.030 cm/cm | 0.010 - 0.030 in/in | |
Multibase TPSiV® 4100-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr.. |
|||
Linear Mold Shrinkage | 0.010 - 0.030 cm/cm | 0.010 - 0.030 in/in | |
Multibase TPSiV® 4100-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr.. |
|||
Linear Mold Shrinkage | 0.010 - 0.030 cm/cm | 0.010 - 0.030 in/in | |
Multibase TPSiV® 4200-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Linear Mold Shrinkage | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Linear Mold Shrinkage | 0.025 - 0.030 cm/cm | 0.025 - 0.030 in/in | |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Linear Mold Shrinkage | 0.015 - 0.030 cm/cm | 0.015 - 0.030 in/in | |
Lehmann & Voss LUVOCOM® 65-8498 PP-copolymer, unreinforced Applications: Office communication.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable for thin wall complex parts.Information provided by Lehmann & Voss &.. |
|||
Linear Mold Shrinkage | 0.018 - 0.030 cm/cm | 0.018 - 0.030 in/in | |
Lehmann & Voss LUVOCOM® 80-8162 Polyacetal-copolymer, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Linear Mold Shrinkage | 0.020 - 0.030 cm/cm @Thickness 3.17 mm |
0.020 - 0.030 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |