Lehmann & Voss LUVOCOM® 1105/WT106 PEEK, unreinforced

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105/WT106 PEEK, unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical resistance parts, non flammable.Inherent flame resistance.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ISO 1183
Water Absorption <= 0.50 %
<= 0.50 %
23°C/24h
Linear Mold Shrinkage 0.010 - 0.016 cm/cm
0.010 - 0.016 in/in
Melt Flow 13.4 g/10 min

@Load 5.00 kg,
Temperature 380 °C
13.4 g/10 min

@Load 11.0 lb,
Temperature 716 °F
Mechanical Properties Metric English Comments
Tensile Stress 100 MPa
14500 psi
Elongation at Yield 5.0 %
5.0 %
6.0 %
6.0 %
flexural
Modulus of Elasticity 3.70 GPa
537 ksi
Flexural Strength 140 MPa
20300 psi
Flexural Modulus 3.00 GPa
435 ksi
Charpy Impact Unnotched 12.0 J/cm²
57.1 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C
27.8 µin/in-°F
DIN 53752
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 250 °C
482 °F
260 °C
500 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 152 °C
306 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color grey white