Bulk Density 0.550 - 0.650 g/cc
0.0199 - 0.0235 lb/in³
Solvay Chemicals Ixper® 60C Calcium Peroxide
IXPER® 60C is a Calcium Peroxide powder used in a wide range of applications in environmental, seed coating, baking e.g. marketsEINECS Number: 215-139-4/CAS Number: 1305-79-9Information provided ..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-VANCE® FR 495 PP copolymer based flame-retardant compound
Fields of application: Injection moulded, or moulded articles (> 1,5 mm thickness) produced via Direct LFT processesExamples: Moulding parts such a under body panels, door modules, industrial parts,..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-VANCE® NU 489 Nucleation masterbatch, PP based
Fields of application: Extruded and injection molded articles made from PP resins.Examples: Extruded PP sheets, films, tapes and blow molded and injection molded articles, such as garden furniture, ..
Bulk Density 0.540 - 0.650 g/cc
0.0195 - 0.0235 lb/in³
Addcomp ADD-VANCE® Start & Stop Shutdown Masterbatch, PP base
Fields of application: Stabilization master batch for polypropylene/polyethylene for stabilization of thermoplastic material in the extruder during shut-down periods to prevent formation of black sp..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-VANCE® TH 130 Stabilization Masterbatch, PP base
Fields of application: Stabilization and processing master batch for producing glass mat reinforced polypropylene (GMT) and long fiber reinforced PP materials (LFTs).Examples: Long fiber reinforced ..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-VANCE® THC 453 PP based masterbatch containing heat stabilizers and carbon black
Fields of application: Stabilization masterbatch for producing long fiber reinforced polypropylene for D-LFT processExamples: Long fiber reinforced pellets to be used for automotive parts, like unde..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-VANCE® THC 723 PP based masterbatch containing heat stabilizers, coupling agent and carbon black
Fields of application: Stabilization masterbatch for producing long fiber reinforced polypropylene for D-LFT and G-LFT processesExamples: Long fiber reinforced polypropylene to be used for automotiv..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-VANCE® THC 732 PP based masterbatch containing heat stabilizers, coupling agent and carbon black
Fields of application: Stabilization masterbatch for producing long fiber reinforced polypropylene for D-LFT and G-LFT processes.Examples: Long fiber reinforced polypropylene to be used for automoti..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-VANCE® THC 831 PP based masterbatch containing heat stabilizers, coupling agent and carbon black
Fields of application: Stabilization masterbatch for producing long fiber reinforced polypropylene for LFT processes.Examples: Long fiber reinforced polypropylene to be used for automotive interior ..
Bulk Density 0.525 - 0.650 g/cc
0.0190 - 0.0235 lb/in³
Addcomp ADD-VANCE® UV 50 20% active PE based anti-UV masterbatch
Fields of application: Foils, films, fibers, extruded and injection molded articles made from PE compatible resins.Examples: Tapes, ropes, carpets, non-wovens, films, fibers, garden furniture, autom..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-MAX® 182 Efficiency masterbatch
Fields of application: Improvement of production efficiency and product qualityExamples: Polyamide 6 and 6,6 staple fibers produced on “short spin” lines.Mode of action and advantages: ADD-MAX 182..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-VANCE® NU 559 Nucleation masterbatch, PP based
Fields of application: Extruded and injection molded articles made from PP and PE resins.Examples: Extruded sheets, films, tapes and blow molded, compression molded and injection molded articles, su..
Bulk Density 0.525 - 0.650 g/cc
0.0190 - 0.0235 lb/in³
Addcomp ADD-VANCE® UV 51 20% active PP based anti-UV masterbatch
Fields of application: Foils, films, fibers, extruded and injection molded articles made from PP compatible resins, like PP, PP/EDPM, PP/PE/EDPM blends (TPOs).Examples: Tapes, ropes, carpets, non-wo..
Bulk Density 0.550 - 0.650 g/cc
0.0199 - 0.0235 lb/in³
Addcomp ADD-VANCE® AS 4030 Anti-static masterbatch, PP based
Fields of application: Anti-static masterbatch for polypropylene.Examples: Thermoformed and injection molded PP products such as margarine containers and other packaging products. Other applications..
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Addcomp ADD-VANCE® FR 243 Halogen-free flame retardant masterbatch, PP based