Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addcomp ADD-VANCE® Start & Stop Shutdown Masterbatch, PP base

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Addcomp
Trade Name ADD-VANCE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-VANCE® Start & Stop Shutdown Masterbatch, PP base.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fields of application: Stabilization master batch for polypropylene/polyethylene for stabilization of thermoplastic material in the extruder during shut-down periods to prevent formation of black spotsExamples: Stabilization of PP/PE in the extruder during shut-down during week-ends or maintenance stops.Mode of action and advantages: ADD-VANCE® Start & Stop is a ready-for-use stabilization masterbatch. ADD-VANCE® Start & Stop contains a synergistic blend of processing stabilizers and heat stabilizers. Processing stabilizers protect the polymer during processing operations at high temperature by decomposing reactive hydroperoxides. Heat stabilizers inhibit the thermooxidative degradation of the end product by radical scavenging reactionAdvantages: Excellent stabilization of thermoplastic polymers. Prevents the development of “black spots” during shut-down and start-up of thermoplastic extruding equipment. Can be processed like general thermoplastic granules, processing conditions (temperatures) do not need to be changed. Non-sticking pellets, dust free dosing. Safe and easy handling, will not damage cylinder, screw, die, and nozzle systems of the machines, even when used repeatedly.Information provided by ADDCOMP
Physical Properties Metric English Comments
Bulk Density 0.540 - 0.650 g/cc
0.0195 - 0.0235 lb/in³
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Descriptive Properties Value Comments
Appearance White to off-white granules
Dosing Level >20%
for stop extuder