Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total Lumicene® MR 2001 Polypropylene, Metallocene Polypropylene ATOFINA Polypropylene MR 2001 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a w.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total Lumicene® MR110MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR110MC2 is a metallocene random copolymer with a melt flow index of 110 g/10 min for injection molding. This Lumicene® MR110MC2 high fluidity differs from standard random copolymers by .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total Lumicene® MR60MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR60MC2 is a metallocene random copolymer with a melt flow index of 60 g/10 min for injection molding. Lumicene® MR60MC2 differs from standard random copolymers by its molding reproducib.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 7642 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7642 is a nucleated and antistatic heterophasic copolymer. PPC 7642 is characterized by a very high stiffness. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 10012 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10012 is a nucleated and antistatic homopolymer polypropylene obtained by controlled rheology.ApplicationPPH 10012 is intended for high speed injection molding of household.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 10042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10042 is a nucleated antistatic homopolymer. PPH 10042 is characterized by high fluidity for high speed injection of thin wall articles such as dairy pots and tubs, salad .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 10099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 1099 is a controlled-rheology homopolymer having a very narrow molecular weight distribution. PPH 10099 is characterized by high fluidity for high speed spinning on spunla.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4026 Polypropylene Homopolymer, Film Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.Polypropylene PPH 4026 is in.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming This grade belongs to the Total Ecosolution line.Polypropylene PPH 4026 is a polypropylene homopolymer specifically developed to offer outstanding processability for sheet extrusion and thermoformin.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4054 Polypropylene Homopolymer Polypropylene PPH 4054 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4054 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4060 is homopolymer.ApplicationATOFINA Polypropylene PPH 4060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 4060 is.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 7069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7069 is homopolymer.ApplicationATOFINA Polypropylene PPH 7069 is characterized by medium fluidity for extrusion of continuous filament (CF) and bulk continuous filament (BC.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9020 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9020 is a clarified homopolymer.ApplicationATOFINA Polypropylene PPH 9020 has been designed with a very high stiffness and an outstanding transparency. It is particularly .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9059 is homopolymer.ApplicationATOFINA Polypropylene PPH 9059 is intended for extrusion of bulk continuous filament (BCF) and continuous filament (CF) fibers. PPH 9059 has.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9081 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPM R021 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R021 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 10222 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10222 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 9220 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 9220 is a nucleated random copolymer polypropylene with a melt flow index of 20 g/10 min for the injection molding of articles with high transparency and excellent surface a.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 60 g/10 min.Polypropylene PPC 11642 is characterized by high fluidity with good mechanical prope.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 2660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 2660 is a heterophasic copolymer. PPC 2660 is characterized by a low fluidity hence good melt strength to provide ease of processing and good manufactured article properti.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 3650 is a heterophasic copolymer with a Melt Flow index of 2 g/10 min.Polypropylene PPC 3650 provides an excellent balance between toughness and flow, being particularly suitable i.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 4663 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4663 is heterophasic copolymer. PPC 4663 is characterized by a combination of ease of processing and good manufacturing article properties in applications ranging from hou.. |
|||
Bulk Density | 0.525 - 0.650 g/cc | 0.0190 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® UV 50 20% active PE based anti-UV masterbatch Fields of application: Foils, films, fibers, extruded and injection molded articles made from PE compatible resins.Examples: Tapes, ropes, carpets, non-wovens, films, fibers, garden furniture, autom.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 3120 MU5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene PPC 3120 MU5 is a heterophasic copolymer with a Melt Flow index of 15 g/10 min. Polypropylene PPC 3120 MU5 is a high impact copolymer formulated to give good UV resistance.Polypropyle.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 3260 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3260 is a random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals. |