Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | Loose |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
Nabaltec APYRAL® 20X Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
Nabaltec APYRAL® 33 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.550 - 0.750 g/cc | 0.0199 - 0.0271 lb/in³ | |
Solvay Chemicals Ixper® 35M Magnesium Peroxide IXPER® 35M is a Magnesium Peroxide powder used in a wide range of applications in environmental, and oil drilling e.g. markets. EINECS Number: 215-627-7/CAS Number: 1335-26-8Information provided .. |
|||
Bulk Density | 0.550 - 0.650 g/cc | 0.0199 - 0.0235 lb/in³ | |
Solvay Chemicals Ixper® 60C Calcium Peroxide IXPER® 60C is a Calcium Peroxide powder used in a wide range of applications in environmental, seed coating, baking e.g. marketsEINECS Number: 215-139-4/CAS Number: 1305-79-9Information provided .. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
Silon PA 0835 HD Processing Aid Concentrate Masterbatch with a highly effective processing aid for polyethylene, especially PE-HD. By using the PA 0835 HD, the output can be markedly increased and the pressure build-up in the barrel decreased.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
Silon Taboradd 23-08350 Processing Aid Masterbatch Masterbatch with a highly effective processing aid for polyethylene, especially PE-X and PE-HD.Information provided by Silon |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | DIN 53466 |
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | DIN 53466 |
Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178 Amber Concentrate Based in LDPE DescriptionPOLYBATCH® Amber 10178 is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178 is designed for use between 3 and 5% HDPE molded bottles (approx. 50 mil) to achieve 90%.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178Z Amber Concentrate Based in LDPE Description POLYBATCH® Amber 10178Z is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178Z is designed for use between 3 and 5% in HDPE molded bottles (approx. 50 mil) to achiev.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | ASTM D1895 |
Plenco 7200 Phenolic, Granular, Injection Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | ASTM D1895 |
Plenco 7487 Phenolic, Granular, Transfer Molded PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178 Amber Concentrate Based in LDPE DescriptionPOLYBATCH® Amber 10178 is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178 is designed for use between 3 and 5% HDPE molded bottles (approx. 50 mil) to achieve 90%.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178Z Amber Concentrate Based in LDPE Description POLYBATCH® Amber 10178Z is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178Z is designed for use between 3 and 5% in HDPE molded bottles (approx. 50 mil) to achiev.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178 Amber Concentrate Based in LDPE DescriptionPOLYBATCH® Amber 10178 is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178 is designed for use between 3 and 5% HDPE molded bottles (approx. 50 mil) to achieve 90%.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178Z Amber Concentrate Based in LDPE Description POLYBATCH® Amber 10178Z is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178Z is designed for use between 3 and 5% in HDPE molded bottles (approx. 50 mil) to achiev.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | ISO 1183 |
Polyram RamClean™ 204 Purging Agent Purging agent for blow molding and extrusion machines.Information provided by Polyram. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 616K PVC PVC Homopolymer General Purpose Grade Resin F616K is a medium-low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178 Amber Concentrate Based in LDPE DescriptionPOLYBATCH® Amber 10178 is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178 is designed for use between 3 and 5% HDPE molded bottles (approx. 50 mil) to achieve 90%.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178 Amber Concentrate Based in LDPE DescriptionPOLYBATCH® Amber 10178 is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178 is designed for use between 3 and 5% HDPE molded bottles (approx. 50 mil) to achieve 90%.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178Z Amber Concentrate Based in LDPE Description POLYBATCH® Amber 10178Z is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178Z is designed for use between 3 and 5% in HDPE molded bottles (approx. 50 mil) to achiev.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | ASTM D1895 |
Plenco 7523 Phenolic, Granular, Transfer Molded PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by P.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178 Amber Concentrate Based in LDPE DescriptionPOLYBATCH® Amber 10178 is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178 is designed for use between 3 and 5% HDPE molded bottles (approx. 50 mil) to achieve 90%.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
A. Schulman POLYBATCH™ 10178Z Amber Concentrate Based in LDPE Description POLYBATCH® Amber 10178Z is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178Z is designed for use between 3 and 5% in HDPE molded bottles (approx. 50 mil) to achiev.. |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
Daikin NEOFLON EC-6520 ETFE Coating Powder, White Description: 0.1-0.3 mm thickness.Processing Methods:Electro-static spray coating.Information provided by Daikin Industries. |
|||
Bulk Density | >= 0.550 g/cc | >= 0.0199 lb/in³ | |
Chosun Refractories A-4 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | |
BASF AH-Salt Recommended use: For the production of homopolymerisates and copolymerisatesInformation provided by BASF |
|||
Bulk Density | 0.550 g/cc | 0.0199 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
Bulk Density | 0.550 - 0.650 g/cc | 0.0199 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® AS 4030 Anti-static masterbatch, PP based Fields of application: Anti-static masterbatch for polypropylene.Examples: Thermoformed and injection molded PP products such as margarine containers and other packaging products. Other applications.. |