Addcomp ADD-VANCE® TH 130 Stabilization Masterbatch, PP base

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Addcomp
Trade Name ADD-VANCE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-VANCE® TH 130 Stabilization Masterbatch, PP base.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fields of application: Stabilization and processing master batch for producing glass mat reinforced polypropylene (GMT) and long fiber reinforced PP materials (LFTs).Examples: Long fiber reinforced materials for automotive parts, like undercover shields, dashboard carriers, assembly carriers, front panels, front bumpers etc.Mode of action and advantages: ADD-VANCE® TH 130 contains a synergistic blend of processing stabilizers and heat stabilizers. Processing stabilizers protect the polymer during processing operations at high temperature by decomposing reactive hydroperoxides. Heat stabilizers inhibit the thermo-oxidative degradation of the end-product by radical scavenging reactions.Advantages: Excellent Long Term Heat Ageing (LTHA) to achieve VW and D-C requirements; Good glueing properties; Non-blooming additives and low emission of organic compounds from finished part; High accuracy in dosing of each individual additive component in ADD-VANCE® TH 130 to ensure product consistency and a guaranteed, defined composition in the final product; Optimized combination of additives to achieve lower overall costs and easy processing; Non-sticking pellets, dust free dosing; Safe and easy handling.Information provided by ADDCOMP
Physical Properties Metric English Comments
Bulk Density 0.500 - 0.650 g/cc
0.0181 - 0.0235 lb/in³
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Descriptive Properties Value Comments
Appearance White to off-white granules
Dosing Level 2-4%