Addcomp ADD-VANCE® AS 4030 Anti-static masterbatch, PP based

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Addcomp
Trade Name ADD-VANCE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-VANCE® AS 4030 Anti-static masterbatch, PP based.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fields of application: Anti-static masterbatch for polypropylene.Examples: Thermoformed and injection molded PP products such as margarine containers and other packaging products. Other applications are films, sheets, tapes, yarns, fibers and household products.Mode of action and advantages: ADD-VANCE AS 4030 contains a high concentration of a highly effective synergistic blend of anti-static additives. The combination of internal anti-static agents used in this product reduces the surface resistance of polypropylene.Advantages: Immediate anti-static protection after production of the PP article; The balanced ratio of fast and controlled migrating anti-static additives does not only provide a rapid anti-static effect but also a prolonged protection against dust attraction and other inconveniences caused by electrostatic charging; Surface resistance of less than 1011 Ohm within 24 hours @ 1% dosing rate; Safe to use as a result of the food contact approved anti-static formulation; Excellent de-moulding properties for injection molded products; Good cost economy; Non-sticking pellets, dust free dosing; and Safe and easy handling.Regulations: ADD-VANCE AS 4030 is very suitable for food packaging products as the active ingredients are in compliance with current food contact regulationsInformation provided by ADDCOMP
Physical Properties Metric English Comments
Bulk Density 0.550 - 0.650 g/cc
0.0199 - 0.0235 lb/in³
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+11 ohm

@Time 86400 sec
<= 1.00e+11 ohm

@Time 24.0 hour
1% dosing rate
Processing Properties Metric English Comments
Processing Temperature <= 280 °C
<= 536 °F
Descriptive Properties Value Comments
Appearance White/off-white granules
Dosing Level 0.4-1.5%