Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Total Atofina
Trade Name Lumicene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® MR 2001 Polypropylene, Metallocene Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATOFINA Polypropylene MR 2001 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a web that is then thermally bonded to manufacture products for hygienic and technical uses.ApplicationATOFINA Polypropylene MR 2001 has a special ant gas-fading formulation to reduce yellowing in fibers.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Flexural Modulus 1.30 GPa
189 ksi
ISO 527-2
Thermal Properties Metric English Comments
Melting Point 151 °C
304 °F
ISO 3146