Material Notes:
ATOFINA Polypropylene PPH 10012 is a nucleated and antistatic homopolymer polypropylene obtained by controlled rheology.ApplicationPPH 10012 is intended for high speed injection molding of household articles, lightweight dairy tubs and goblets and ice cream boxes. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 42 g/10 min

@Load 2.16 kg,
Temperature 230 °C
42 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ISO 2039-2
Tensile Strength, Yield 34.0 MPa
4930 psi
ISO 527-2
Elongation at Yield 9.0 %
9.0 %
ISO 527-2
Tensile Modulus 1.60 GPa
232 ksi
ISO 527-2
Flexural Modulus 1.50 GPa
218 ksi
ISO 527-2
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
120°C per hour; ISO 75-2
Vicat Softening Point 87.0 °C
189 °F
50N-50°C per hour; ISO 306
152 °C
306 °F
10N-50°C per hour; ISO 306