Material Notes:
Polypropylene PPM R021 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the exclusion of implants. This grade can also be injection molded.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc
0.902 g/cc
ISO 1183
Bulk Density 0.525 g/cc
0.0190 lb/in³
ISO 1183
Melt Flow 1.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ISO 2039-2
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527-2
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-2
Flexural Modulus 0.900 GPa
131 ksi
ISO 179
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 149 °C
300 °F
ISO 3146
Vicat Softening Point 67.0 °C

@Load 5.10 kg
153 °F

@Load 11.2 lb
50°C per hour; ISO 306
130 °C

@Load 1.02 kg
266 °F

@Load 2.25 lb
50°C per hour; ISO 306