Polymer Property : Density = 0.0788 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.15 - 2.18 g/cc
0.0777 - 0.0788 lb/in³
DIN 53479
Fluorseals PTFE Unfilled
Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Density 2.14 - 2.18 g/cc
0.0773 - 0.0788 lb/in³
ASTM D792
Guarniflon PTFE G400 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Density 2.14 - 2.18 g/cc
0.0773 - 0.0788 lb/in³
ASTM D792
Guarniflon PTFE G800 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Density 2.13 - 2.18 g/cc
0.0770 - 0.0788 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance..
Density 2.13 - 2.18 g/cc
0.0770 - 0.0788 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Density 2.13 - 2.18 g/cc
0.0770 - 0.0788 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Density 2.13 - 2.18 g/cc
0.0770 - 0.0788 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Density 2.13 - 2.18 g/cc
0.0770 - 0.0788 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Density 2.13 - 2.18 g/cc
0.0770 - 0.0788 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer
Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f..
Density 2.10 - 2.18 g/cc
0.0759 - 0.0788 lb/in³
BS2782:Pt6
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite
Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is..
Density 2.10 - 2.18 g/cc
0.0759 - 0.0788 lb/in³
BS2782:Pt6
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite
Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is..