Material Notes:
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarniflon®
Physical Properties Metric English Comments
Density 2.14 - 2.18 g/cc
0.0773 - 0.0788 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength >= 24.0 MPa
>= 3480 psi
extruded; ASTM D4894
>= 30.0 MPa
>= 4350 psi
molded; ASTM D4894
Elongation at Break >= 300 %
>= 300 %
extruded; ASTM D4894
>= 400 %
>= 400 %
molded; ASTM D4894
Compressive Yield Strength 5.00 - 6.00 MPa

@Strain 1.00 %
725 - 870 psi

@Strain 1.00 %
ASTM D695
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 40.0 kV/mm
>= 1020 kV/in
in air, extruded; ASTM D149
>= 60.0 kV/mm
>= 1520 kV/in
in air, molded; ASTM D149