Material Notes:
PCTFE is a high performance crystalline polymer with excellent chemical resistance. Because of its low moisture absorption, PCTFE can operate in a continuous service temperature of -250°F to 300°F.Typical Applications:Bearings and BushingsBall Valve SeatsSemiconductor Processing EquipmentGearsTanksElectrical ComponentsPump PartsHydraulic ComponentsGasketsCircuit BoardsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 2.14 g/cc
0.0773 lb/in³
ASTM D792
Filler Content 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ASTM D2240
Tensile Strength 42.1 MPa
6100 psi
ASTM D638
Elongation at Break 37 %
37 %
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Izod Impact, Notched 0.758 J/cm
1.42 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Continuous
Minimum Service Temperature, Air -157 °C
-250 °F
Continuous
Descriptive Properties Value Comments
Color White
Users viewing this material also viewed the following: