Multibase Multibatch® MP 50004 Anti-split

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multibatch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multibatch® MP 50004 Anti-split.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HPP. 70% CaCO3 Filled.Thermal Resistance.Information provided by Multibase
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
ISO R 1183
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 230 °C
10 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133