Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Konduit
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP KONDUIT PX11311U PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermally conductive mineral and glass fiber filled PA6 compliant with ECO protocols, non-brominated, non chlorinated
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
5 mm/min; ISO 527
Elongation at Break 1.7 %
1.7 %
5 mm/min; ISO 527
Tensile Modulus 12.5 GPa
1810 ksi
1 mm/min; ISO 527
Flexural Yield Strength 170 MPa
24700 psi
2 mm/min; ISO 178
Flexural Modulus 11.0 GPa
1600 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
34.6 µm/m-°C

@Temperature -30.0 - 80.0 °C
19.2 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
37.2 µm/m-°C

@Temperature 23.0 - 80.0 °C
20.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 47.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
60.4 µm/m-°C

@Temperature -30.0 - 80.0 °C
33.6 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
73.4 µm/m-°C

@Temperature 23.0 - 80.0 °C
40.8 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
through-plane, ø80*3mm discs; ISO 22007-2
1.30 W/m-K
9.02 BTU-in/hr-ft²-°F
in-plane, ø80*3mm discs; ISO 22007-2
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
365 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 205 °C
401 °F
Rate B/120; ISO 306
Flammability, UL94 V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Comparative Tracking Index >= 600 V
>= 600 V
UL 746A
600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2