Physical Properties Metric English Comments
Density 1.24 - 1.29 g/cc

@Temperature 250 - 295 °C
0.0448 - 0.0466 lb/in³

@Temperature 482 - 563 °F
Average value: 1.26 g/cc Grade Count:7
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Density 1.05 - 1.29 g/cc
0.0379 - 0.0466 lb/in³
Average value: 1.14 g/cc Grade Count:29
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Density 1.26 - 1.29 g/cc
0.0455 - 0.0466 lb/in³
309-1D Resin
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive
Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh..
Density 1.21 - 1.29 g/cc
0.0437 - 0.0466 lb/in³
OSTM059
Solvay TOLCIDE® PS 50A 50% tetrakis hydroxymethyl phosphonium sulfate
Identification: PROPRIETARY FORMULATION BASED ON TETRAKIS (HYDROXYMETHYL) PHOSPHONIUM SULPHATE (THPS) BLENDED WITH A NOVEL POLYMERIC PERFORMANCE ENHANCER.Function: Industrial biocidal productBiodegr..
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds CL 64 Flexible PVC, Sheathing
Good flexibility at low temperatures
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds FK 001/AL Flexible PVC, Insulation Lead Free
General purposes suitable for food contact according to CEE 90/128
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds GS 7512 Flexible PVC, Injection Molding for Footwear
Soles
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds GS 6020 Flexible PVC, Injection Molding for Footwear
High boots
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds GS 6520 Flexible PVC, Injection Molding for Footwear
Soles
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds PH 70/AS Flexible PVC, Transparent Extrusion
Food belt carriers
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds PH 75/AS Flexible PVC, Transparent Extrusion
Food belt carriers
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds PHS 75/B Flexible PVC, Transparent Extrusion
Pipes for gasoline CAVIS
Density 1.03 - 1.29 g/cc
0.0372 - 0.0466 lb/in³
Average value: 1.13 g/cc Grade Count:91
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Density 1.12 - 1.29 g/cc
0.0405 - 0.0466 lb/in³
Average value: 1.19 g/cc Grade Count:26
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..