Sika Industry SikaFlex 252 One Part Polyurethane Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Sika Industry
Trade Name SikaFlex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sika Industry SikaFlex 252 One Part Polyurethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sika 252 SikaFlex One Part Polyurethane AdhesiveA high viscous, high strength adhesive, this product can replace rivets, screws, welds, and other mechanical fasteners. Seals and bonds in one step. 4 mm Cut-Off. Available in black, white, gray. Good non-sag. Cure Type: Moisture
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0420 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 50
45 - 50
Tensile Strength, Ultimate 3.79 - 4.48 MPa
550 - 650 psi
Elongation at Break 550 - 650 %
550 - 650 %
Adhesive Bond Strength 2.41 - 2.76 MPa
350 - 400 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.6 °C
195 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 - 45.0 min
0.500 - 0.750 hour
Tack-free
1440 min
24.0 hour
Value given per 3/16 inches
Shelf Life 9.00 Month
9.00 Month