Material Notes:
PC0798 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0798 is a halogenated, colorable, chemically crosslinkable copolymer compound which contains flame retardant additives to reduce normal flame spread characteristics so as to achieve a flame resistant rating when used according to the UL 44 Horizontal test on 14 AWG. Specifications Underwriters Laboratories Standards 44 and 854.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 11.1 MPa
>= 1610 psi
after aging (168h, 150°C); ASTM D412
13.1 MPa
1900 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 23 %
23 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Dielectric Constant 2.6

@Frequency 60000 Hz
2.6

@Frequency 60000 Hz
ASTM D150
Dielectric Strength >= 550 kV/mm
>= 14000 kV/in
ASTM D149
Dissipation Factor 0.0025

@Frequency 60000 Hz
0.0025

@Frequency 60000 Hz
ASTM D150
Processing Properties Metric English Comments
Middle Barrel Temperature 116 - 127 °C
241 - 261 °F
Melt Temperature 127 °C
261 °F
Back Pressure 1.72 MPa
249 psi
steam pressure
Shelf Life 18.0 Month
18.0 Month