Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cast Nylons Nycast® XHA Heat Stabilized Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Cast
Manufacturer Cast Nylons Limited
Trade Name Nycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cast Nylons Nycast® XHA Heat Stabilized Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat stabilized Cast Nylon 6 adds up to 20 degrees F higher continuous operation temperature for those applications that require additional temperature resistance beyond the standard resistance. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values presented for comparison purposes. Actual property values may differ.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
24 hrs; ASTM D570
Water Absorption at Saturation 5.5 %
5.5 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Hardness, Shore D 77
77
ASTM D2240
Tensile Strength, Ultimate 88.0 MPa
12800 psi
ASTM D638
Elongation at Break 20 - 30 %
20 - 30 %
ASTM D638
Tensile Modulus 2.90 GPa
421 ksi
ASTM D638
Flexural Yield Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Compressive Modulus 2.10 GPa
305 ksi
ASTM D695
Shear Strength 72.0 MPa
10400 psi
ASTM D732
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 81.0 µm/m-°C

@Temperature 20.0 °C
45.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Maximum Service Temperature, Air 121 °C
250 °F
Continuous service
166 °C
331 °F
Intermittent service
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 166 - 204 °C
331 - 399 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved