Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.70 - 3.75 g/cc | 0.134 - 0.135 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9510 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.70 - 3.80 g/cc | 0.134 - 0.137 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9612 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.70 - 3.75 g/cc | 0.134 - 0.135 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9620 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.70 - 3.80 g/cc | 0.134 - 0.137 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 115 TC Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 325 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 615-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 625-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.71 g/cc | 0.134 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 725-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | |
NanoScale NanoActive® Titanium Dioxide NanoActive TiO2 is produced using proprietary processes to obtain high specific surface area (over 500 m²/g), high porosity, weakly aggregated, amorphous material possessing adsorption capacity and.. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | |
MarkeTech Repton EXP 383 Alumina 96% REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 3.72 g/cc | 0.134 lb/in³ | |
GBC Grade 97 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | |
Misumi Alumina 96 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
Density | 3.71 g/cc | 0.134 lb/in³ | |
Indium Corp. Indalloy 186 Germanium-Aluminum Solder Alloy Information Provided by Indium Corporation |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | |
Schott N-PK52A Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Density | 3.71 g/cc | 0.134 lb/in³ | |
Schott N-SSK5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | ASTM D792 |
Techmer ES Electrablend® PPS 06000 Availability: North AmericaForms: PelletsFiller/Reinforcement: Metallic FlakeFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | |
Sapco 95% Aluminum Oxide Information provided by Sapco. |
|||
Density | 3.72 g/cc | 0.134 lb/in³ | ASTM C20 |
CoorsTek AD-96 Alumina (nom. 96% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 3.72 g/cc | 0.134 lb/in³ | ASTM-C373 |
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | ASTM-C 20 |
CoorsTek Z-PLUS™ 94 Zirconia-Impr. Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |
|||
Density | >= 3.70 g/cc | >= 0.134 lb/in³ | |
Advanced Ceramics ALC 1082 (C-786) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring.. |
|||
Density | 3.70 g/cc | 0.134 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec 614/698 Alumina, 96% 614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink. |
|||
Density | 3.72 g/cc | 0.134 lb/in³ | DIN EN 623-2 |
CeramTec Rubalit® IS 95 Brown Alumina Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at.. |
|||
Density | 3.70 - 4.40 g/cc | 0.134 - 0.159 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 551.059 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni) |
|||
Density | 3.70 - 4.40 g/cc | 0.134 - 0.159 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 551.074 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni) |
|||
Density | 3.70 - 4.40 g/cc | 0.134 - 0.159 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 551.088 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni) |