Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.72 g/cc | 0.134 lb/in³ | |
GBC Grade 97 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Density | 3.72 g/cc | 0.134 lb/in³ | ASTM C20 |
CoorsTek AD-96 Alumina (nom. 96% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 3.72 g/cc | 0.134 lb/in³ | ASTM-C373 |
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |
|||
Density | 3.72 g/cc | 0.134 lb/in³ | DIN EN 623-2 |
CeramTec Rubalit® IS 95 Brown Alumina Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at.. |