Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 3.70 g/cc
0.134 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Liner
76.2 microns
3.00 mil
Carrier
381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
Silicone Property; ASTM D2240
Tensile Strength 3.34 MPa
485 psi
Silicone Property; ASTM D412
Elongation at Break 60 %
60 %
Silicone Property; ASTM D412
Modulus of Elasticity 0.01957 GPa
2.838 ksi
ASTM E 831
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Modulus 0.000379 GPa
0.0550 ksi
ASTM D 1002
Shear Strength 3.65 MPa
530 psi
Lap Shear Strength; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 93.0 µm/m-°C
51.7 µin/in-°F
Silicone Property; ASTM E 831
Specific Heat Capacity 0.400 J/g-°C
0.0956 BTU/lb-°F
E 1461-01
Thermal Conductivity 0.750 W/m-K
5.20 BTU-in/hr-ft²-°F
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg <= -100 °C
<= -148 °F
Silicone Property; ASTM D3418
Electrical Properties Metric English Comments
Volume Resistivity 500 ohm-cm
500 ohm-cm
Silicone Property; ASTM D991
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 141 °C
0.250 hour

@Temperature 285 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature -15.0 - -9.44 °C
6.00 Month

@Temperature 5.00 - 15.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Naturally Gray
Total Product Weight (g/m2) 1410
Arlon SQA-TMS-025