Nabaltec GRANALOX® NM 9510 F Ceramic Body

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Nabaltec GmbH
Trade Name GRANALOX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec GRANALOX® NM 9510 F Ceramic Body.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum are tailored to the application areas in which the material is used such as wear resistance, high temperature stability, good electrical insulation, thermal conductivity and corrosion resistance.Used in machinery parts and ballistic ceramics.Information provided by Nabaltec.
Physical Properties Metric English Comments
Bulk Density 1.20 - 1.35 g/cc
0.0434 - 0.0488 lb/in³
Density 3.70 - 3.75 g/cc
0.134 - 0.135 lb/in³
Sintered
Moisture Absorption at Equilibrium 0.10 - 0.40 %
0.10 - 0.40 %
Loss On Ignition 5.6 %
5.6 %
Particle Size 70 - 120 µm
70 - 120 µm
Mean Granulate Size
Thermal Properties Metric English Comments
Shrinkage 14.5 - 15.5 %
14.5 - 15.5 %
linear
Component Elements Properties Metric English Comments
Al2O3 95 %
95 %
Na2O 0.10 %
0.10 %
Processing Properties Metric English Comments
Sintering Temperature 1550 - 1650 °C
2820 - 3000 °F
Interval (dense ceramic parts)
1600 °C

@Time 7200 sec
2910 °F

@Time 2.00 hour