Density 3.65 - 3.75 g/cc
0.132 - 0.135 lb/in³
Sintered Density
Nabaltec GRANALOX® NM 9212 F Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.70 - 3.75 g/cc
0.134 - 0.135 lb/in³
Sintered
Nabaltec GRANALOX® NM 9510 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.70 - 3.75 g/cc
0.134 - 0.135 lb/in³
Sintered Density
Nabaltec GRANALOX® NM 9620 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..