CoorsTek Z-PLUS™ 94 Zirconia-Impr. Alumina Ceramic Armor Material

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer CoorsTek
Trade Name Z-PLUS™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek Z-PLUS™ 94 Zirconia-Impr. Alumina Ceramic Armor Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor systems with proven ballistic performance for National Institute of Justice (N.I.J.) and international design standards(C).
Physical Properties Metric English Comments
Density 3.70 g/cc
0.134 lb/in³
ASTM-C 20
Mechanical Properties Metric English Comments
Hardness, Rockwell 45 N 78
78
Modulus of Elasticity 303 GPa
43900 ksi
ASTM-C848
Flexural Strength 352 MPa
51100 psi
MOR; ASTM-F417
Compressive Strength 2103 MPa
305000 psi
ASTM-C773
Poissons Ratio 0.21
0.21
ASTM-C848
Fracture Toughness 4.00 - 5.00 MPa-m½
3.64 - 4.55 ksi-in½
Klc; Notched Beam
Shear Modulus 125 GPa
18100 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
Thermal Conductivity 22.4 W/m-K
155 BTU-in/hr-ft²-°F
ASTM-C408