Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring S2260Product Use: Electrically conductive electronic adhesive. Bonds with primer.Appearance: Naturally (gray) colored, high viscosity gum (tan or brown after cure)This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 3.70 g/cc
0.134 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Liner
76.2 microns
3.00 mil
Carrier
102 microns
4.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Silicone Property; ASTM D2240
Tensile Strength 2.65 MPa
385 psi
Silicone Property; ASTM D412
Elongation at Break 225 %
225 %
Silicone Property; ASTM D412
Modulus of Elasticity 0.00550 GPa
0.798 ksi
Silicone Property; Arlon-SAQ-TMS-008
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Modulus 0.000296 GPa
0.0430 ksi
ASTM D1002
Shear Strength 2.76 MPa
400 psi
Lap Shear Strength; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 93.0 µm/m-°C
51.7 µin/in-°F
ASTM E 831
Specific Heat Capacity 0.400 J/g-°C
0.0956 BTU/lb-°F
Silicone Property; E1461-01
Thermal Conductivity 2.50 W/m-K
17.4 BTU-in/hr-ft²-°F
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg -116 °C
-177 °F
Silicone Property; ASTM E 1356
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 0.050 ohm-cm
0.050 ohm-cm
Silicone Property; ASTM D991
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 141 °C
0.250 hour

@Temperature 285 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 4.44 - 10.0 °C
6.00 Month

@Temperature 40.0 - 50.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Naturally Gray
Total Product Weight (g/m2) 376