Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrablend® PPS 06000

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Conductive
Manufacturer Techmer ES
Trade Name Electrablend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® PPS 06000.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Metallic FlakeFeatures: Electrically ConductiveInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 3.70 g/cc
0.134 lb/in³
ASTM D792
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 µm/m-°C
11.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 274 °C
525 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.399 mm
V-0

@Thickness 0.0157 in
Electrical Properties Metric English Comments
Volume Resistivity 1.0 ohm-cm
1.0 ohm-cm
ASTM D257
Surface Resistance 1.0 ohm
1.0 ohm
ASTM D257