Physical Properties Metric English Comments
Density 1.70 - 1.73 g/cc
0.0614 - 0.0625 lb/in³
Liquid
Oceanchem Group Calcium Bromide (CaBr2)
Molecular Formula: CaBr2Cas No.: 7789-41-5Use: Calcium Bromide and its formuulated brines are mainly used as completion, workover and packer fluids in oil drilling field.Properties: This product is ..
Density 1.13 - 1.73 g/cc
0.0408 - 0.0625 lb/in³
Average value: 1.30 g/cc Grade Count:55
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Density 1.20 - 1.73 g/cc
0.0434 - 0.0625 lb/in³
Average value: 1.51 g/cc Grade Count:35
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Density 1.16 - 1.73 g/cc
0.0419 - 0.0625 lb/in³
Average value: 1.38 g/cc Grade Count:70
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Density 1.18 - 1.73 g/cc
0.0426 - 0.0625 lb/in³
Average value: 1.33 g/cc Grade Count:5
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
Density 1.23 - 1.73 g/cc
0.0444 - 0.0625 lb/in³
Average value: 1.45 g/cc Grade Count:117
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Density 1.25 - 1.73 g/cc
0.0452 - 0.0625 lb/in³
Average value: 1.53 g/cc Grade Count:50
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..