Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.18 - 1.73 g/cc
0.0426 - 0.0625 lb/in³
Average value: 1.33 g/cc Grade Count:5
Linear Mold Shrinkage 0.00200 - 0.00950 cm/cm
0.00200 - 0.00950 in/in
Average value: 0.00675 cm/cm Grade Count:4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.0 - 105 MPa
8700 - 15200 psi
Average value: 84.8 MPa Grade Count:3
Elongation at Break 1.50 - 8.00 %
1.50 - 8.00 %
Average value: 5.83 % Grade Count:3
Flexural Yield Strength 110 - 165 MPa
16000 - 24000 psi
Average value: 136 MPa Grade Count:3
Flexural Modulus 3.30 - 7.60 GPa
479 - 1100 ksi
Average value: 4.83 GPa Grade Count:4
Izod Impact, Notched (ISO) 3.00 - 8.50 kJ/m²
1.43 - 4.04 ft-lb/in²
Average value: 6.00 kJ/m² Grade Count:3
Thermal Properties Metric English Comments
Melting Point 200 - 260 °C
392 - 500 °F
Average value: 234 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 127 - 235 °C
261 - 455 °F
Average value: 178 °C Grade Count:5