Physical Properties Metric English Comments
Density 1.15 - 1.17 g/cc
0.0415 - 0.0423 lb/in³
Polymerized; ASTM D792
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Density 1.16 - 1.17 g/cc
0.0419 - 0.0423 lb/in³
Polymerized; ASTM D792
Proto3000 Objet TangoGray FullCure950 Rubber-like Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Density 1.03 - 1.17 g/cc

@Temperature 250 - 250 °C
0.0372 - 0.0423 lb/in³

@Temperature 482 - 482 °F
Average value: 1.10 g/cc Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Density 0.940 - 1.17 g/cc
0.0340 - 0.0423 lb/in³
Average value: 1.03 g/cc Grade Count:41
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Density 1.07 - 1.17 g/cc
0.0387 - 0.0423 lb/in³
Average value: 1.11 g/cc Grade Count:4
Overview of materials for Nylon 11 with Graphite Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with Graphite Filler". Each property range of values reported is minimum and maximum values of ..
Density 1.05 - 1.17 g/cc
0.0379 - 0.0423 lb/in³
Average value: 1.07 g/cc Grade Count:7
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..
Density 1.125 - 1.17 g/cc
0.04064 - 0.0423 lb/in³
OSTM059
Solvay AQUARITE® ESL Surfactant
Identification: PHOSPHONATE END CAPPED SULPHONATED COPOLYMERAvailable in: Asia Pacific, Europe, Latin America and North America. Applications: AQUARITE® ESL is a patented, high performance, broad..
Density 1.13 - 1.17 g/cc
0.0408 - 0.0423 lb/in³
ISO R 1183
Fainplast Compounds GS 39/T Flexible PVC, Injection Molding for Footwear
Sandals
Density 1.13 - 1.17 g/cc
0.0408 - 0.0423 lb/in³
ISO R 1183
Fainplast Compounds GS 46/T Flexible PVC, Injection Molding for Footwear
Vamp boots
Density 1.13 - 1.17 g/cc
0.0408 - 0.0423 lb/in³
ISO R 1183
Fainplast Compounds GS 65/R-AS Flexible PVC, Injection Molding for Footwear
Oil resistent and antistatic soles
Density 1.15 - 1.17 g/cc
0.0416 - 0.0423 lb/in³
ASTM D792
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6)
Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo..
Density 1.13 - 1.17 g/cc
0.0408 - 0.0423 lb/in³
ISO R 1184
Fainplast Compounds MPH 50/T Medical Flexible PVC, Extrusion
Technical tubes and peristaltic pump segments no DOP
Density 1.13 - 1.17 g/cc
0.0408 - 0.0423 lb/in³
ISO R 1183
Fainplast Compounds PH 45/1 Flexible PVC, Transparent Extrusion
Transparent profiles
Density 1.13 - 1.17 g/cc
0.0408 - 0.0423 lb/in³
Internal
AKG Polymers Vision PP PPH BL1303 G30 Polypropylene Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Density 1.13 - 1.17 g/cc
0.0408 - 0.0423 lb/in³
ISO 1183
Austin Novel Materials Texalan® 590A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Density 1.15 - 1.17 g/cc
0.0415 - 0.0423 lb/in³
AdvanSource Biomaterials HydroMed™ D640 Permanently Lubricious Polyurethane Coating
AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether hydrophilic polyurethanes designed for use as coatings of catheters, sutures, in..
Density 1.15 - 1.17 g/cc
0.0415 - 0.0423 lb/in³
AdvanSource Biomaterials HydroSlip™ C Hydrophilic Polyether Aliphatic Polyurethane
AdvanSource Biomaterials Corporation manufactures and markets thermoplastic elastomeric hydrogels under the tradename HydroThane™. HydroThane™ is a generic family of polyurethane hydrogels, with ..
Density 0.679 - 1.17 g/cc
0.0245 - 0.0423 lb/in³
Average value: 1.14 g/cc Grade Count:63
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Density 1.08 - 1.17 g/cc
0.0390 - 0.0423 lb/in³
Average value: 1.13 g/cc Grade Count:13
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim..
Density 1.01 - 1.17 g/cc
0.0365 - 0.0423 lb/in³
Average value: 1.13 g/cc Grade Count:64
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Copyright © lookpolymers.com All Rights Reserved