Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company CP710 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer M. Holland Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company CP710 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AntistaticImpact copolymerGood flowGood impact resistanceNucleatedApplications: ClosuresHousehold goodsThin-walled parts
Physical Properties Metric English Comments
Density 0.901 g/cc
0.0326 lb/in³
ASTM D1505
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
73°F; ASTM D256
Descriptive Properties Value Comments
Characteristics Antistatic, Nucleating agent
Forms Pellets
Processing Methods Injection molding
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved