Bapolene® PP5052 Polypropylene, Injection Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® PP5052 Polypropylene, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene injection impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA standards for food contact applications.Applications: Battery cases, housewares, appliances.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.903 g/cc
0.0326 lb/in³
ASTM D1505
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
ASTM D-2240
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 160 %
160 %
2 in/min (50 mm/min); ASTM D638
Elongation at Yield 14 %
14 %
2 in/min (20 mm/min); ASTM D638
Flexural Modulus 1.21 GPa
175 ksi
Secant @ 1% strain; ASTM D-790
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
183 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution