Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.120 g/cc | 0.00434 lb/in³ | Free Rise Density |
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or machine casting by the meter dispensing equipment. The components are stable and liquid at .. |
|||
Density | 0.120 - 0.150 g/cc | 0.00434 - 0.00542 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® C70.130 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |
|||
Density | 0.120 - 0.160 g/cc | 0.00434 - 0.00578 lb/in³ | ASTM D792 |
Microcell Composite Company CELLIFF® F-1020ST Polymer Foam CELLIFF® FOAM is Light & rigid, tenacious & durable. Patterns can be easily molded into the foam surface. We possess the technology to increase surface hardness to meet requirement.Information pr.. |
|||
Density | 0.120 g/cc | 0.00434 lb/in³ | |
Sawbones Cellular Rigid Polyurethane Foam 7.5 pcf Density Cellular Rigid Polyurethane FoamPrimary UseCellular rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. Its outward appearance matches cancellous bone .. |
|||
Density | 0.120 - 0.140 g/cc | 0.00434 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Siliconcell 414/0 Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Density | 0.120 - 0.180 g/cc | 0.00434 - 0.00650 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 302/T-E NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |