Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.110 - 0.140 g/cc | 0.00397 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLIFF® F7010 Polymer Foam CELLIFF® FOAM is Light & rigid, tenacious & durable. Patterns can be easily molded into the foam surface. We possess the technology to increase surface hardness to meet requirement.Information pr.. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLOMER® S-2110 SBS Rubber Foam CELLOMER® FOAM is non-toxic, contains no heavy metal, PVC-free, chloride-free, light weight, superior-grip in wet & dry, high elasticity & resilience. Can be 100% recycled.Information provided by.. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLOMER® S-2110D SBS Rubber Foam CELLOMER® FOAM is non-toxic, contains no heavy metal, PVC-free, chloride-free, light weight, superior-grip in wet & dry, high elasticity & resilience. Can be 100% recycled.Information provided by.. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLAMP® M5010 Thermoplastic Foam CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high.. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 301/F NR-SBR Foam Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-RS EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.120 - 0.140 g/cc | 0.00434 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Siliconcell 414/0 Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-BI EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-KPA 45 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | |
3M K1 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-GR EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLAMP® M5110 Thermoplastic Foam CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high d.. |