Eurofoam Siliconcell 414/0 Silicone Foam

Category Polymer , Thermoset , Silicone , Silicone Foam
Manufacturer Eurofoam s.r.l.
Trade Name Siliconcell
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Siliconcell 414/0 Silicone Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.120 - 0.140 g/cc
0.00434 - 0.00506 lb/in³
ISO 845-88
Mechanical Properties Metric English Comments
Tensile Strength 0.200 MPa
29.0 psi
ASTM D 412
Elongation at Break >= 200 %
>= 200 %
ASTM D 412
Compressive Yield Strength 0.00800 MPa

@Strain 25.0 %
1.16 psi

@Strain 25.0 %
ASTM 1056/85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
ASTM D 3575
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
ASTM D 3575
Descriptive Properties Value Comments
Cellular Structure Open
Color Brown
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC