Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Microcell Composite Company CELLIFF® F-1020ST Polymer Foam

Category Polymer
Manufacturer Microcell Composite Company
Trade Name CELLIFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Microcell Composite Company CELLIFF® F-1020ST Polymer Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CELLIFF® FOAM is Light & rigid, tenacious & durable. Patterns can be easily molded into the foam surface. We possess the technology to increase surface hardness to meet requirement.Information provided by Microcell Composite Company
Physical Properties Metric English Comments
Density 0.120 - 0.160 g/cc
0.00434 - 0.00578 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 78 - 82
78 - 82
ASTM D2240
Tensile Strength, Yield 2.94 MPa
427 psi
ASTM D412
Elongation at Yield 150 %
150 %
ASTM D412
Tear Strength 14.7 kN/m
84.0 pli
ASTM D624
Compression Set 85 %

@Temperature 70.0 °C,
Time 21600 sec
85 %

@Temperature 158 °F,
Time 6.00 hour
50%; ASTM D395
Thermal Properties Metric English Comments
Shrinkage 5.0 %

@Temperature 70.0 °C,
Time 2400 sec
5.0 %

@Temperature 158 °F,
Time 0.667 hour
ASTM D1204
Descriptive Properties Value Comments
Resiliency (%) 55
ASTM D2632
Users viewing this material also viewed the following: